Superconducting powder
Our company offers YBa2Cu3O7-x (YBCO) powder with different degrees of dispersion – from 1 μm to 100 μm. The critical temperature for powders TC is 90-92 К.
Powder parameters are stable and provide increased production quality by pressing and annealing.
Minimal order 100 gram.
The fraction is selected by mechanical separation.
Range of powder dispersion YBCO
|
Price per 100 grams, USD.
|
150-100 μm in a mixture with smaller dimensions without separation
|
440
219
|
100-60 μm
|
560
279
|
60-30 μm
|
580
349
|
30 μm in a mixture with smaller dimensions
|
665
399
|